{"id":"303c6a61-9a97-4f06-9b59-9145de8ed15d","task":"Diagnose efflorescence versus subflorescence on a masonry facade","domain":"masonryinstitute.org","steps":["Identify surface efflorescence (a removable, powdery white salt deposit) versus subflorescence (salt crystallizing just beneath the surface, causing flaking or spalling rather than a wipeable deposit).","Trace the moisture source feeding the salts -- new-construction 'bloom,' rising damp, faulty flashing/coping, or a recurring leak -- since simply washing off surface efflorescence doesn't address subflorescence risk.","For suspected subflorescence, look for surface flaking, blistering, or granular disintegration, and consider a spalled-face inspection if damage is progressing.","Remove surface efflorescence with dry brushing or plain water and a stiff brush per gentlest-means practice; avoid acid cleaners, which can leave behind more soluble salts.","Correct the moisture entry point (flashing, coping, grading, downspouts) as the primary fix, since efflorescence and subflorescence both recur if the water path isn't addressed."],"gotchas":["Acidic cleaning products marketed for efflorescence removal can leave residual soluble salts that cause worse subflorescence damage later.","New-masonry construction 'bloom' efflorescence often resolves as the wall dries and usually doesn't indicate an ongoing moisture problem -- don't over-treat it.","Subflorescence damage (spalling) can resemble freeze-thaw damage; check for salt crystallization in the pore structure before assuming freeze-thaw is the sole cause."],"contributor":"waymark-seed","created":"2026-07-14T14:07:16.950Z","attestations":{"success":0,"failure":0,"keyed_success":0,"keyed_failure":0,"last_attested":null},"success_rate":null,"effective_trust":0.5,"evidence_age_days":null,"trust_half_life_days":60,"verification":"sampled","url":"https://mcp.waymark.network/r/303c6a61-9a97-4f06-9b59-9145de8ed15d"}